Chemical Composition
Special wax
Technical Parameters
Nature of the wax | Twax-967 | |
Appearance | White Powder | |
Particle size μm | ||
Dv50 | 4 | |
Dv90 | 8 | |
Melting point ℃ | 115 |
Characteristics and Purposes
Ø Twax-967 with very uniform particle size, easy to disperse, with high hardness, good on smoothness, special modified to ensure the product with stable and ultrafine particle size.
Ø Especially suitable for the thin coating, the feature of concentrate and fine particle size, can greatly reduce the flowing defect of thin coating
Ø Very suitable for can coating, easy to disperse, with high smoothness and excellent on abrasion resistance, scratch resistance.
Ø With very good dispersion and storage stability when used in wood coating, provide very flat coating surface, has excellent transparency and obvious scratch resistance effect, with very good smooth feeling.
Ø Can be used in paint, printing ink, leather those solvent and non solvent systems, it is good on dispersion stability, provide excellent hand feeling and scratch resistance.
Ø Can be used in powder coating, will not smoke and has very good effect on scratch resistance, and is helpful on increasing the fluidity of powder coating.
Contents and Methods of Use
Ø In a variety of systems, the additional amount of the micronized wax is generally between 0.5 to 3%.
Ø Usually by a direct high-speed stirring, it can disperse in solvent-based coatings and printing inks.
Ø It can be added by a variety of grinding machines, high-shear dispersing device, and should pay attention to the temperature control when using the grind mill.
Ø Can carry out the decentralized processing to make the wax slurry with the wax powder concentration at 20-30%., then add it into the systems when needed, which can decrease the dispersion time.
Packaging and Storage
Ø Drum, net weight: 20kg / barrel.
Ø This product is non-dangerous goods. Please store it away from ignition sources and strong oxidants.