Heat stabilizer2018-12-27
This series of polyethylene wax products can effectively improve the fluidity of PVC heat stabilizer processing, increase the extrusion efficiency of PVC products, and improve the surface gloss of products. They can also effectively control the agglomeration of PVC heat stabilizer processing and effectively solve the precipitation of PVC heat stabilizer processing.
The important application of PE wax lies in PVC processing. Compared with fatty acid lubricants, it has no adverse effects on melt tension and Vicat softening point, and provides excellent anti-adhesion and flow control. PE wax can be used to control melting in a special process. Even if the amount of addition is large, it has a very good compatibility with other components.PE wax is the only one of the known plastic lubricants that possesses both internal and external lubrications (demolding ef...
PVC profiles2018-12-27
Wax for PVC profiles can increase the extrusion efficiency of PVC products, improve the surface gloss of PVC products, and can effectively enhance the plasticization degree of PVC products processing system.Wax for PVC profile has low viscosity, high softening point, good hardness, non-toxicity, good thermal stability, low high-temperature volatility and other performance. As a lubricant, it has stable chemical properties and good electrical properties.Wax for PVC profiles can increase the gloss...