Leather polishing process is divided into three steps: coarse polishing, medium polishing and fine polishing. To get the best effect, good polishing wax must be selected. Tianshi polishing wax has high brightness, easy to polish, with good gloss, able to replace carnauba wax. It can also be used in water-based system.
Leather plating release wax, a kind of water-based environment-friendly nonionic wax, features acid resistance, alkali resistance, hard water resistance, strong water solubility, fine particle size and stable performance. When applied to the leather surface, it has very good plating release to prevent the plate from sticking under high temperature plate pressing, and won't affect the bonding between coatings, and can provide the leather with smooth, soft, and full feel.
Burnish wax2018-12-27
It is a kind of water-soluble and environment-friendly anionic burn wax, adopting advanced synthetic wax as the main raw material, with strong water solubility and stable emulsion, without holes on the surface or precipitation on the bottom, and able to be diluted in any proportion without stratification and demulsification. After using this, the leather surface is endowed with intense burn effect and high glossiness.
This kind of wax is used when the leather's original wax layer, maintenance layer and anti-fouling layer are thoroughly cleaned. The waterborne burn polish wax possesses uniform color and high temperature resistance, able to be used in the pre-treatment synthetic leather process. It can also be used in solvent system due to its good abrasive resistance.
Oily wax2018-12-27
Tianshi wax can provide leather with a slippery feel, with good stability and good transparency, not easy to precipitate.
Polish wax2018-12-27
The wax has a polishing effect in the leather, making the leather brighter and naturally shiny, able to polish rub and burn. Some wax products of Tianshi can substitute carnauba wax, and can be used in the water-based system.
Pull up wax2018-12-27
Tianshi wax is used for the pull-up treatment of the artificial leather surface, with uniform particle size and strong discoloration effect, easy to disperse.
Pull-up wax2018-12-27
Tianshi wax can provide the leather surface with pull up effect, environment-friendly, with high temperature resistance, able to be used in water-based system.