Bonding agent2018-12-27
Waxes in powder coating have bonding agent. The micronized wax does not dissolve under the temperature of bonding, which can be coated on powder coating particles to prevent them from sticking together. Compared with inorganic materials, wax powder as a bonding separator will not affect the leveling of powder coatings.
Another function of waxes in powder coatings is degassing or defoaming. They are often used as a defoaming agent for coatings, which can solve the pinholes and depressions of porous substrates. The relative wax products of Tianshi have superior pollution resistance, extremely low additive amount and little impact on gloss.
Hardening agent2018-12-27
Hardening agent: the following waxes can be used in powder coatings, mainly to improve product surface hardness, scratch resistance and coating surface smoothness.
The relative wax products of Tianshi can create sand texture effect, easy to disperse and can modify a variety of materials, with rich sand texture effects, fine sandy feel and smooth feel, can improve extrusion effect.